Facile synthesis of CuCr2O4/BiOBr nanocomposite and its photocatalytic activity towards RhB and tetracycline hydrochloride degradation under household visible LED light irradiation

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
5

Citation Types

0
8
0

Year Published

2021
2021
2023
2023

Publication Types

Select...
8

Relationship

0
8

Authors

Journals

citations
Cited by 36 publications
(8 citation statements)
references
References 75 publications
0
8
0
Order By: Relevance
“…The formation of the BiOBr@G composite is further confirmed through Raman spectroscopy, and the resulting Raman spectrum is shown in Figure b. The A 1g internal stretching mode of Bi-Br in BiOBr corresponds to the strong Raman band appearing at 112.2 cm –1 . , Additionally, no obvious Raman signals are observed around 1346 or 1595 cm –1 for pure BiOBr. A characteristic peak of BiOBr is also observed at 114.5 cm –1 for the BiOBr@G composite.…”
Section: Resultsmentioning
confidence: 78%
See 1 more Smart Citation
“…The formation of the BiOBr@G composite is further confirmed through Raman spectroscopy, and the resulting Raman spectrum is shown in Figure b. The A 1g internal stretching mode of Bi-Br in BiOBr corresponds to the strong Raman band appearing at 112.2 cm –1 . , Additionally, no obvious Raman signals are observed around 1346 or 1595 cm –1 for pure BiOBr. A characteristic peak of BiOBr is also observed at 114.5 cm –1 for the BiOBr@G composite.…”
Section: Resultsmentioning
confidence: 78%
“…The A 1g internal stretching mode of Bi-Br in BiOBr corresponds to the strong Raman band appearing at 112.2 cm −1 . 26,27 Additionally, no obvious Raman signals are observed around 1346 or 1595 cm −1 for pure BiOBr. A characteristic peak of BiOBr is also observed at 114.5 cm −1 for the BiOBr@G composite.…”
Section: Resultsmentioning
confidence: 93%
“…The results exhibited typical IV-type adsorption-desorption isotherm curves with an H3 hysteresis loop, suggesting that all the catalysts feature meso-porous structures. 6,37,38 Table 1 provides information on the surface area, pore volume, and typical pore diameter. The BET surface areas of BiOBr, PbMoO 4 , and PMB-3 are 18.69 m 2 g À1 , 22.27 m 2 g À1 , and 12.2 m 2 g À1 , respectively.…”
Section: Resultsmentioning
confidence: 99%
“…The results exhibited typical IV-type adsorption–desorption isotherm curves with an H3 hysteresis loop, suggesting that all the catalysts feature meso-porous structures. 6,37,38…”
Section: Resultsmentioning
confidence: 99%
“…The Al 2p orbital located at 74.56 eV can be assigned to the Al–O–Cu bond of CuAl 2 O 4 by the high resolution Cr 2p spectrum of spinel CuCr 2 O 4 oxides as shown in Figure S1e. The binding energies at 576.46, 578.59, and 582.73 eV belong to the Cr 2p3/2 orbital, while the binding energies at 586.30 and 588.47 eV belong to the Cr 2p1/2 orbital, corresponding to Cr 3+ ion in CuCr 2 O 4 oxides. , Figure S1h shows the Fe 2p spectrum of spinel CuFe 2 O 4 oxides. The binding energies at 710.49 and 712.92 eV represent Fe 2p3/2, whereas the binding energies at 724.07 and 726.46 eV are for Fe 2p1/2 of Fe 3+ and the two satellite peaks at 718.64 and 733.89 eV are attributed to Fe 3+ in CuFe 2 O 4 oxides …”
Section: Resultsmentioning
confidence: 99%