2021
DOI: 10.1016/j.jestch.2021.02.013
|View full text |Cite
|
Sign up to set email alerts
|

Exploring the influence of process parameters on the properties of SiC/A380 Al alloy surface composite fabricated by friction stir processing

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
4
1

Citation Types

1
10
0

Year Published

2021
2021
2024
2024

Publication Types

Select...
8
2

Relationship

0
10

Authors

Journals

citations
Cited by 18 publications
(14 citation statements)
references
References 30 publications
1
10
0
Order By: Relevance
“…The hardness and wear resistance were analyzed in surface composite of A380-SiC using FSP route. The optimum values of hardness (177 Hv) at 1460 tool rpm during FSP-ed surface composite and wear rate (4x10-8 gm/cm) was noted at 15 N loading conditions as concluded by Maryam and Akeel 21) . To the authors knowledge, few reports are explored to fabricate the Al6063/graphene nano powder SCs using FSP technique.…”
Section: Introductionsupporting
confidence: 53%
“…The hardness and wear resistance were analyzed in surface composite of A380-SiC using FSP route. The optimum values of hardness (177 Hv) at 1460 tool rpm during FSP-ed surface composite and wear rate (4x10-8 gm/cm) was noted at 15 N loading conditions as concluded by Maryam and Akeel 21) . To the authors knowledge, few reports are explored to fabricate the Al6063/graphene nano powder SCs using FSP technique.…”
Section: Introductionsupporting
confidence: 53%
“…FSP technology is also successfully used to eliminate defects and material loss in the sample [ 14 ] and to produce surface composites [ 15 , 16 , 17 ] or to modify the microstructure of composites [ 18 , 19 ]. The production of surface composites consists in introducing the reinforcing phase in the form of particles [ 20 , 21 , 22 ] or fibers [ 23 ] into the plasticized matrix. Currently, there are a number of solutions and methods allowing effective introduction of the reinforcing phase during FSP and the production of a surface composite [ 24 ].…”
Section: Introductionmentioning
confidence: 99%
“…Additionally, the decrease in hardness below the base metal value was less present on the retreating side. Such non-symmetrical behavior can mostly be attributed to the temperature increase in the advancing side in comparison to the retreating side during processing, as reported by [40,41]. The hardness profile recorded for the workpiece processed with a plunge depth of 0.6 mm was reported by Sharma et al [26], indicating steep fluctuations in the hardness values from the center towards the composite/matrix interface.…”
Section: Microhardnessmentioning
confidence: 69%