Effects of Ionic Strength in the Medium on Sample Preconcentration Utilizing Nano-interstices between Self-Assembled Monolayers of Gold Nanoparticles

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1

Citation Types

0
4
0

Year Published

2019
2019
2024
2024

Publication Types

Select...
5
1

Relationship

1
5

Authors

Journals

citations
Cited by 7 publications
(4 citation statements)
references
References 25 publications
0
4
0
Order By: Relevance
“…Salinization on the substrate surface was achieved using a (3-aminopropyl) triethoxysilane (APTES) mixture solution/H 2 O with a volume ratio of 1:1000 for 1 min. The APTES silanization and AuNPs self-assembly processes have been reported in our previous publications [34,38,39,40]. The obtained results indicated that the salinization duration of 1 min was suitable.…”
Section: Methodsmentioning
confidence: 54%
See 1 more Smart Citation
“…Salinization on the substrate surface was achieved using a (3-aminopropyl) triethoxysilane (APTES) mixture solution/H 2 O with a volume ratio of 1:1000 for 1 min. The APTES silanization and AuNPs self-assembly processes have been reported in our previous publications [34,38,39,40]. The obtained results indicated that the salinization duration of 1 min was suitable.…”
Section: Methodsmentioning
confidence: 54%
“…Gold beads with a mean diameter of 13 nm, purchased from Taiwan Advanced Nanotech Inc., were used in this study. The AuNPs diameter of 13 ± 1 nm was also chosen as the optimal size in our previous works for the protein preconcentrators [34,38,39,40]. Figure 3b–d shows the SAMs of AuNPs on a gold–glass substrate captured by a scanning electron microscopy system at magnifications of 20,000, 100,000, and 200,000 times, separately.…”
Section: Resultsmentioning
confidence: 99%
“…This differs considerably from MAP containing nano-particles or micro-particles in solution where ionic strength must be considered. 16 In traditional MAPs, the CIP are embedded in a PDMS matrix and make up between 10 and 90 wt% of the mass of the entire mixture. 1 In this work, a much lower CIP concentration is employed, and the PDMS matrix is relatively soft (Shore A00 hardness).…”
Section: Sample Fabrication and Preparationmentioning
confidence: 99%
“…CIP SQ has a pure iron (Fe) content of up to 99,8%. This differs considerably from MAP containing nano‐particles or micro‐particles in solution where ionic strength must be considered . In traditional MAPs, the CIP are embedded in a PDMS matrix and make up between 10 and 90 wt% of the mass of the entire mixture .…”