Effect of the composition and conditions of the synthesis of porous glass on their micro- and mesoporous structures

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1

Citation Types

0
3
0

Year Published

2016
2016
2023
2023

Publication Types

Select...
8

Relationship

0
8

Authors

Journals

citations
Cited by 14 publications
(3 citation statements)
references
References 19 publications
0
3
0
Order By: Relevance
“…GC chemical composition is the following: 0.25 Na 2 O – 3.42 B 2 O 3 – 96.09 SiO 2 – 0.24 Ag 2 O. The sample preparation is a complex and multi-stage procedure, which includes PG fabrication that is based on two-phase alkali borosilicate glass thermal treatment and the following chemical etching to delete a borate phase [ 21 , 22 ]. The final impregnation procedure with silver/copper halides is described elsewhere [ 23 ].…”
Section: Materials Laser Procedures and Modellingmentioning
confidence: 99%
“…GC chemical composition is the following: 0.25 Na 2 O – 3.42 B 2 O 3 – 96.09 SiO 2 – 0.24 Ag 2 O. The sample preparation is a complex and multi-stage procedure, which includes PG fabrication that is based on two-phase alkali borosilicate glass thermal treatment and the following chemical etching to delete a borate phase [ 21 , 22 ]. The final impregnation procedure with silver/copper halides is described elsewhere [ 23 ].…”
Section: Materials Laser Procedures and Modellingmentioning
confidence: 99%
“…To obtain porous glass materials the following methods are used: through chemical etching (leaching) of two-phase glass with interpenetrating phases [ 16 ], the sol-gel method [ 17 ], template synthesis method [ 18 ] and replica method [ 19 ], which consists in sequential mixing of glass powder, solution for impregnation of the polymer matrix with further high temperature treatment of the finished mixture. The disadvantages of these methods are rather strict limitations on the pore size.…”
Section: Introductionmentioning
confidence: 99%
“…In this work, two-phase alkali-borosilicate (ABS) glass of three compositions with the plant heat treatment [3] ) (NK-3, the heat treatment is 550°С 30 h) in the form of plates of 15 × 15 × 2 mm were exposed to leaching in acid-salt solutions in order to eliminate the chemically unstable phase according to the procedure described in [4]. The PG whose compositions are given in Table 1 were investigated on the content of Lewis basic and Brøn-sted acidic centers on the internal surface of the PG (the PG specimens were assigned individual designations) (Table 2).…”
mentioning