Effect of Die Head Temperature at Compounding Stage on the Degradation of Linear Low Density Polyethylene/Plastic Film Waste Blends after Accelerated Weathering

Abstract: Accelerated weathering test was performed on blends of linear low density polyethylene (LLDPE) and plastic film waste constituting the following percentages of polyolefin polymers (wt.%): LLDPE (46%), low density polyethylene (LDPE, 51%), high density polyethylene (HDPE, 1%), and polypropylene (PP, 2%). Compounded blends were evaluated for their mechanical and physical (optical) properties. The impact of photodegradation on the formulated blends was studied, and loss of mechanical integrity was apparent with r… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1
1

Citation Types

1
16
0

Year Published

2019
2019
2024
2024

Publication Types

Select...
4
2
2

Relationship

0
8

Authors

Journals

citations
Cited by 25 publications
(25 citation statements)
references
References 45 publications
(76 reference statements)
1
16
0
Order By: Relevance
“…It is also worth mentioning that various implications, touching base on sustainability and plastic waste pollution, fall within the framework of this study. The developed film blends originating from PSW, have proven their viability as a standalone produce comparable to ones on the market [33,34,54]. This also supports the claim that freshly discarded PSW with somewhat preserved integrity, allows the development of plastic film blends with acceptable market standards.…”
Section: Resultssupporting
confidence: 54%
See 2 more Smart Citations
“…It is also worth mentioning that various implications, touching base on sustainability and plastic waste pollution, fall within the framework of this study. The developed film blends originating from PSW, have proven their viability as a standalone produce comparable to ones on the market [33,34,54]. This also supports the claim that freshly discarded PSW with somewhat preserved integrity, allows the development of plastic film blends with acceptable market standards.…”
Section: Resultssupporting
confidence: 54%
“…The material was segregated and cleaned for further processing [33]. The PSW contained the following polymer as constituting elements (by wt%): LLDPE (46%), LDPE (51%), HDPE (1%); and PP (2%) [34]. The PSW was milled to 3 mm flakes using a Tecnova cutting mill and pelletized to 3 mm pellets using a Tecnova single screw extruder (L/D = 30) at 40 bars pressure and 70 rpm.…”
Section: Methodsmentioning
confidence: 99%
See 1 more Smart Citation
“…In general, lightness (L*) was in line with the general colour measurement theory, since transparent and achromatic films should have high lightness and minimum colour space values of a * and b*. Al-Salem et al [27], [28] also tested colour parameters of control unexposed LLDPE/Waste (100/0) sample extruded using a single screw extruder (L/D=30) and film blowing machine. The reported L*, a* and b* values were 29.0, -0.4, and -3.5, respectively.…”
Section: Methodsmentioning
confidence: 76%
“…The equipment used was cleaned every 800 h to remove scale deposits resulting from water evaporation during the condensation cycles. Readers are referred to Al-Salem et al [7], [8], [14] for a detailed depiction on the accelerated weathering procedure.…”
Section: Accelerated Ageing Of Test Specimensmentioning
confidence: 99%