Differential scanning calorimetry/small-angle X-ray scattering analysis of ultraviolet sensible polypropylene filaments

Abstract: In this work, ultraviolet (UV) sensible metallocene isotactic polypropylene (miPP) filaments were produced with different drawing ratios and various concentrations of photochromic pigment. The effects of pigment concentration and drawing ratio on the chromatic properties and the structural modification for the miPP filaments were studied extensively by differential scanning calorimetry (DSC) and small- and wide-angle X-ray scattering (SAXS/WAXS) measurements. The change in melting temperature and the polymeric… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1

Citation Types

0
1
0

Year Published

2022
2022
2024
2024

Publication Types

Select...
4
1

Relationship

2
3

Authors

Journals

citations
Cited by 5 publications
(2 citation statements)
references
References 38 publications
0
1
0
Order By: Relevance
“…By incorporating more biobased fibers, including natural and regenerated fibers, as well as other biobased and biodegradable polymers, it is possible to mitigate the overall pollution burden on wastewater treatment plants. Furthermore, the application of mass coloring or mass functionalization in the process of melt extrusion, namely in the case of polylactic acid, or in manmade fibers like viscose, infinna, spinnova, renewcell and ioncel has the potential to decrease the pollution burden associated with both synthetic and regenerate fibers [336][337][338][339].…”
Section: Discussionmentioning
confidence: 99%
“…By incorporating more biobased fibers, including natural and regenerated fibers, as well as other biobased and biodegradable polymers, it is possible to mitigate the overall pollution burden on wastewater treatment plants. Furthermore, the application of mass coloring or mass functionalization in the process of melt extrusion, namely in the case of polylactic acid, or in manmade fibers like viscose, infinna, spinnova, renewcell and ioncel has the potential to decrease the pollution burden associated with both synthetic and regenerate fibers [336][337][338][339].…”
Section: Discussionmentioning
confidence: 99%
“…Fibers such as silk and viscose rayon could be lustrous and they influence capturing the image and followed by the image processing. Some of the fibers have special dyes such as photo and thermochromic dyes have a strong influence on the identification [ 168 , 169 , 170 , 171 ]. Additionally, optical brighteners, optical brightening agents (OBAs), fluorescent brightening agents (FBAs), or fluorescent whitening agents (FWAs) are typically applied to white fabrics in order to improve their brightness and whiteness [ 172 , 173 , 174 ].…”
Section: Machine Vision Can Control the Microfiber Releasesmentioning
confidence: 99%