2013
DOI: 10.1007/s10570-013-0057-6
|View full text |Cite
|
Sign up to set email alerts
|

Development of antimicrobial cotton fabric using bionanocomposites

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1
1
1

Citation Types

2
7
0

Year Published

2015
2015
2022
2022

Publication Types

Select...
8
1

Relationship

0
9

Authors

Journals

citations
Cited by 24 publications
(9 citation statements)
references
References 39 publications
2
7
0
Order By: Relevance
“…) as shown in Fig.5. This result agrees with the result found byAltınışık et al, (Altınışık et al, 2013) for cellulosic fibre. The crystallinity percentages of 60g/L, 70g/L, 80g/L, 90g/L, and 100g/L FC-dendrimer-treated samples were 81.44, 79.98, 80.76, 79.83, and 77.931, respectively.…”
supporting
confidence: 93%
“…) as shown in Fig.5. This result agrees with the result found byAltınışık et al, (Altınışık et al, 2013) for cellulosic fibre. The crystallinity percentages of 60g/L, 70g/L, 80g/L, 90g/L, and 100g/L FC-dendrimer-treated samples were 81.44, 79.98, 80.76, 79.83, and 77.931, respectively.…”
supporting
confidence: 93%
“…The ICP analysis of silver nanoparticle-coated cotton fabric was carried out using a Jobin-YVON—JV-138 ULTR (Made in France) instrument. The silver particle concentration was calculated from the calibration curve of standard solutions as was reported (Altınısık et al, 2013; Nourbakhsh & Ashjaran, 2012). The antibacterial activity and concentration of silver particles on sputtered cotton samples after 10 times of washing with repeated home laundering according to American Association of Textile Chemists and Colorists (AATCC) Test Method 124-1996 were also investigated.…”
Section: Methodsmentioning
confidence: 99%
“…The accelerating voltage was 5-12 kV. The fabricated samples were prepared for SEM analysis by coating the surface with gold [19].…”
Section: Scanning Electron Microscopy (Sem)mentioning
confidence: 99%