2015
DOI: 10.4314/tjpr.v14i2.4
|View full text |Cite
|
Sign up to set email alerts
|

Development and In vitro Evaluation of Self-Adhesive Matrix-Type Transdermal Delivery System of Ondansetron Hydrochloride

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

0
6
0

Year Published

2017
2017
2024
2024

Publication Types

Select...
7
2
1

Relationship

0
10

Authors

Journals

citations
Cited by 18 publications
(7 citation statements)
references
References 13 publications
0
6
0
Order By: Relevance
“…Likewise, similar observations were made with other Eudragit polymer grades (RSPO/RLPO) of D and E series patches. A tensile strength of 4 MPa and above is desirable for transdermal patches according to the American Society for Testing and Materials (ASTM) guidelines (23). The data revea led that the average tensile strength of all the patches was in the range of 4.09 to 9.98 MPa, indicating good tensile strength.…”
Section: Thickness and Tensile Strengthmentioning
confidence: 77%
“…Likewise, similar observations were made with other Eudragit polymer grades (RSPO/RLPO) of D and E series patches. A tensile strength of 4 MPa and above is desirable for transdermal patches according to the American Society for Testing and Materials (ASTM) guidelines (23). The data revea led that the average tensile strength of all the patches was in the range of 4.09 to 9.98 MPa, indicating good tensile strength.…”
Section: Thickness and Tensile Strengthmentioning
confidence: 77%
“…The capability of a polymeric nanocomposite film to uptake moisture content from the environment is considered to affect the release rate of the drug from the system. 28 The formulations were subjected to moisture uptake test by weighing each film initially and keeping it in a desiccator containing a saturated solution of sodium chloride. The weight of each film was measured after every 24 hours until a constant weight was achieved.…”
Section: Methodsmentioning
confidence: 99%
“…The polymeric matrix patches were prepared by solvent casting methods by dissolving 400 mg of Eudragit RS 100 and 300 mg of EC in 5 mL of chloroform with the help of slow magnetic stirrer in a beaker. 11 – 13 Also, 100 mg of copolymer (PVP) and 3 mL of silicone adhesive were added with uniform stirring. Then, to the above solution, DBS plasticizer at 20% of the total polymer weight and 20–40 mg of MP were added and stirred for 30 min.…”
Section: Methodsmentioning