Cu-implanted ZnO nanorods array film: An aqueous synthetic approach

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1
1

Citation Types

0
5
0

Year Published

2015
2015
2024
2024

Publication Types

Select...
5
1

Relationship

2
4

Authors

Journals

citations
Cited by 7 publications
(5 citation statements)
references
References 49 publications
0
5
0
Order By: Relevance
“…In this connection, ZnO is considered as one of the most important nanostructured materials 1 in nanotechnology because of its structure richness and novel properties. To date, various morphologies of ZnO have been synthesized such as nanobelts, 2 nanocombs, 3 nanosheets, 4 nanocages, 5 nanorings, 6 needle-like nanowhiskers, 7 nanorods 8,9 and nanoforest. 10 These morphologies have variety of practical applications which motivated the researchers towards controllable synthesis of ZnO nano-architectures.…”
Section: Introductionmentioning
confidence: 99%
“…In this connection, ZnO is considered as one of the most important nanostructured materials 1 in nanotechnology because of its structure richness and novel properties. To date, various morphologies of ZnO have been synthesized such as nanobelts, 2 nanocombs, 3 nanosheets, 4 nanocages, 5 nanorings, 6 needle-like nanowhiskers, 7 nanorods 8,9 and nanoforest. 10 These morphologies have variety of practical applications which motivated the researchers towards controllable synthesis of ZnO nano-architectures.…”
Section: Introductionmentioning
confidence: 99%
“…The various vibrational bands arised for CdS structure i.e. one broad peak in the region of 3300e3600 cm À1 centered at 3419.99 cm À1 and one weak peak at around 1628.62 cm À1 was due to stretching and bending vibration of OeH group respectively [19,23]. Peaks appeared at 2854.25 and 2924.24 cm À1 corresponds to CeH stretch vibration.…”
Section: Resultsmentioning
confidence: 97%
“…All PEC studies were carried out in 0?5M Na 2 SO 4 (pH 6?8) solution, which served as supporting electrolyte medium. The ZnO/Zn electrode was scanned from 2500 to 1500 mV(Ag/AgCl) at a rate of 5 mV s 21 . Amperometric I-t curves were performed by measuring the current as a function of the time at z0?50 V(Ag/ AgCl).…”
Section: Experimental Preparation Of Zinc Oxide Thin Filmsmentioning
confidence: 99%
“…16 ZnO nanorods, nanowires and nanobelts have extensive application potential in nanogenerators, piezoelectric field effect transistors and chemical sensors, piezoelectric diodes, triggers, transducer and actuator, and flexible piezotronic strain sensors. [17][18][19][20][21] In recent years, there have been many reports on the preparation of ZnO nanorods by thermal evaporation, alumina templates, chemical vapour deposition and electrochemical deposition. [22][23][24][25] However, these preparation methods still involve some complex procedures, sophisticated equipment and rigorous experimental conditions.…”
Section: Introductionmentioning
confidence: 99%