Core-shell Fe3O4@SiO2@PANI composite: Preparation, characterization, and applications in microwave absorption

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

1
14
0

Year Published

2022
2022
2024
2024

Publication Types

Select...
10

Relationship

0
10

Authors

Journals

citations
Cited by 60 publications
(18 citation statements)
references
References 45 publications
1
14
0
Order By: Relevance
“…27,28 No other diffraction peaks are found, indicating the high purity of the as-prepared Fe 3 O 4 . 29 Similar to the XRD pattern of Fe 3 O 4 , the XRD pattern of Fe 3 O 4 @ SiO 2 shows the characteristic peaks of Fe 3 O 4 only, which reveals a homogeneous dispersion of the amorphous SiO 2 shell and no other characteristic peaks are found. In the meanwhile, Fe 3 O 4 particles are well retained in the silica matrix with no phase change, indicating the successful preparation of the carrier Fe 3 O 4 @ SiO 2 .…”
Section: Resultssupporting
confidence: 55%
“…27,28 No other diffraction peaks are found, indicating the high purity of the as-prepared Fe 3 O 4 . 29 Similar to the XRD pattern of Fe 3 O 4 , the XRD pattern of Fe 3 O 4 @ SiO 2 shows the characteristic peaks of Fe 3 O 4 only, which reveals a homogeneous dispersion of the amorphous SiO 2 shell and no other characteristic peaks are found. In the meanwhile, Fe 3 O 4 particles are well retained in the silica matrix with no phase change, indicating the successful preparation of the carrier Fe 3 O 4 @ SiO 2 .…”
Section: Resultssupporting
confidence: 55%
“…88-0866), respectively, could be detected for both F-RGO and F-RGO-p-PANI-II. 47 Meanwhile, weak diffraction peaks at 2 θ = 14.9°, 18.4° and 25.38°, corresponding to the (011), (020) and (200) crystal planes of PANI, could also be found in the pattern of the F-RGO-p-PANI-II hybrid. 48…”
Section: Resultsmentioning
confidence: 97%
“…4b). 53 The absorption peaks from 400 cm −1 to 700 cm −1 can be ascribed to Ti-O-Ti and Ti-O telescopic vibration absorption peaks, indicating the formation of TiO 2 layers (Fig. 4c).…”
Section: Computer Simulation Of the Template And Monomer In Mipsmentioning
confidence: 96%