Continuous cooling precipitation diagram of cast aluminium alloy Al-7Si-0.3Mg

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1
1

Citation Types

1
10
0

Year Published

2016
2016
2019
2019

Publication Types

Select...
5
2

Relationship

1
6

Authors

Journals

citations
Cited by 25 publications
(13 citation statements)
references
References 15 publications
1
10
0
Order By: Relevance
“…For this reason, the difference in the solution treatments between Al7Si0.3Mg and Al10Si0.3 should be kept in mind when considering Figure 73. Figure 73 shows that the maximum hardness achievable for the three alloys is very similar (111 to 116 HV1), and this hardness is achieved using high cooling rates in excess of ≈100 K/s [131,214]. This result perfectly fits with those of Ref.…”
Section: Alsimg Cast Alloyssupporting
confidence: 81%
See 2 more Smart Citations
“…For this reason, the difference in the solution treatments between Al7Si0.3Mg and Al10Si0.3 should be kept in mind when considering Figure 73. Figure 73 shows that the maximum hardness achievable for the three alloys is very similar (111 to 116 HV1), and this hardness is achieved using high cooling rates in excess of ≈100 K/s [131,214]. This result perfectly fits with those of Ref.…”
Section: Alsimg Cast Alloyssupporting
confidence: 81%
“…In this work, three variants of AlSiMg cast alloys are assessed, namely permanent mould-cast Al7Si0.3Mg [214], high-pressure die-cast Al10Si0.3Mg [131] and additively manufactured (laser-beam melted, LBM) Al10Si0.3Mg [131]. Figure 69 compares these three cast alloy variants in terms of their DSC cooling curves (A, B) and the resulting precipitation enthalpies and hardness after ageing (C, D).…”
Section: Alsimg Cast Alloysmentioning
confidence: 99%
See 1 more Smart Citation
“…Water has 1.0-1.1 of H value, and oil has 0.30-0.35 of H value [9,14]. The characteristic of water quenching produce non-uniform geometry and high temperature gradient on specimen, which generated the residual stress and the distortion [5]. Al 2 O 3 particle affected distortion of the specimen.…”
Section: Fig 1 Stir Casting Equipmentmentioning
confidence: 99%
“…Quenching rate must be fast to obtain maximum strength of material. On the other hand, quenching rate must be slow to avoid the distortion [5].…”
Section: Introductionmentioning
confidence: 99%