2013
DOI: 10.1016/j.compositesb.2012.05.020
|View full text |Cite
|
Sign up to set email alerts
|

Composites based on carbon black reinforced NBR/EPDM rubber blends

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
2
1

Citation Types

4
62
0
4

Year Published

2015
2015
2023
2023

Publication Types

Select...
8
1

Relationship

0
9

Authors

Journals

citations
Cited by 120 publications
(70 citation statements)
references
References 26 publications
4
62
0
4
Order By: Relevance
“…During the deformation process, the movement of molecular chain and the stress transformed is limited. 35 Therefore, the composite modulus consistently increases with increasing particle loading since many interactions between polymer segments and inorganic fillers are produced. It is also concluded that these materials exhibited similar human skin-like behavior, as the elastic modulus (E 0 ) was measured to be 1.13, 1.5, 1.83, and 2.17 MPa for PDMS and 30, 50, and 70 wt % carbonyl iron materials, respectively.…”
Section: Resultsmentioning
confidence: 98%
“…During the deformation process, the movement of molecular chain and the stress transformed is limited. 35 Therefore, the composite modulus consistently increases with increasing particle loading since many interactions between polymer segments and inorganic fillers are produced. It is also concluded that these materials exhibited similar human skin-like behavior, as the elastic modulus (E 0 ) was measured to be 1.13, 1.5, 1.83, and 2.17 MPa for PDMS and 30, 50, and 70 wt % carbonyl iron materials, respectively.…”
Section: Resultsmentioning
confidence: 98%
“…The blends were compounded using a Haake Polylab OS Rheodrive 16 internal mixer with a Banbury rotor at 0.70 fill factor and with overall 50 g of each blend formulation. The ratio of NR/EPDM, amount of EPDM-g-MAH compatibilizer, and internal mixer machine parameters had been optimized prior to this work and were reported elsewhere [39,42,43]. The melt-blending operation was performed at a mixing temperature of 70°C and rotor speed of 70 rpm for 5 min.…”
Section: Characterization Of Ugnps and Gnps-peimentioning
confidence: 99%
“…The first heating endotherms were analyzed to understand the influence of GNPs modification and amount of loading to the heat flow behavior of the produced blends. The glass transition temperature (T g ) was determined from the primary point that intersected the tangent discontinuity in the DSC curve [43].…”
Section: Characterization Of Ugnps and Gnps-peimentioning
confidence: 99%
“…These are called surface functional groups. These surface functional groups increase the chemical and physical bonding between the CBs particles and the rubber matrix [39][40][41][42][43].…”
Section: Introductionmentioning
confidence: 99%