2004
DOI: 10.1016/j.scriptamat.2004.01.010
|View full text |Cite
|
Sign up to set email alerts
|

Cold rolling textures in AZ31 wrought magnesium alloy

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1
1
1

Citation Types

9
118
1
2

Year Published

2006
2006
2018
2018

Publication Types

Select...
5
5

Relationship

0
10

Authors

Journals

citations
Cited by 371 publications
(161 citation statements)
references
References 7 publications
9
118
1
2
Order By: Relevance
“…The double-peak texture of (0002) plane has been reported in the other studies. 18,19) It is noted that the texture intensities of the route 2, route 3 and route 4 specimens were weaker than that of the route 1 specimen, and in particular, the texture intensities of the route 3 and route 4 specimens were approximately half of that of the route 1 specimen. The fact that the route 2, route 3 and route 4 specimens showed lower texture intensities than the route 1 specimen is probably related to the deference in plastic flow during rolling, as shown in Fig.…”
Section: Resultsmentioning
confidence: 99%
“…The double-peak texture of (0002) plane has been reported in the other studies. 18,19) It is noted that the texture intensities of the route 2, route 3 and route 4 specimens were weaker than that of the route 1 specimen, and in particular, the texture intensities of the route 3 and route 4 specimens were approximately half of that of the route 1 specimen. The fact that the route 2, route 3 and route 4 specimens showed lower texture intensities than the route 1 specimen is probably related to the deference in plastic flow during rolling, as shown in Fig.…”
Section: Resultsmentioning
confidence: 99%
“…The texture of the fraction of deformed grains forms a basal alignment parallel to the sheet plane, as well as a TD spread. This is associated with a six-peak symmetry of the prismatic planes, which is often associated with prismatic slip [24] along similar strain paths. The latter feature is also developed after deformation with geometry VII; however, the TD spread does not appear.…”
Section: Microstructure Development During Formingmentioning
confidence: 99%
“…11. The (00.2) pole figures of the extruded Mg processed by 1/8 turn of HPT exhibits double textures, which indicates the non-basal <c+a> slip is activated along with the basal slip [48,49 ].…”
Section: Deformation Mechanisms Of Mg During Hptmentioning