2015
DOI: 10.1016/j.indcrop.2015.07.006
|View full text |Cite
|
Sign up to set email alerts
|

Cellulose fibers isolated from energycane bagasse using alkaline and sodium chlorite treatments: Structural, chemical and thermal properties

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
2
1

Citation Types

3
38
0

Year Published

2015
2015
2024
2024

Publication Types

Select...
7

Relationship

1
6

Authors

Journals

citations
Cited by 104 publications
(41 citation statements)
references
References 36 publications
3
38
0
Order By: Relevance
“…This finding was in agreement with Yue et al (2015). The removal of hemicellulose with the borax treatment was validated by FTIR analysis.…”
Section: Determination Of Chemical Components Of Treated and Untreatesupporting
confidence: 88%
See 2 more Smart Citations
“…This finding was in agreement with Yue et al (2015). The removal of hemicellulose with the borax treatment was validated by FTIR analysis.…”
Section: Determination Of Chemical Components Of Treated and Untreatesupporting
confidence: 88%
“…These bands were attributed to the C=O stretching of carbonyl groups of hemicellulose or lignin. The disappearance of these peaks in the borax-treated fibers explained the considerable removal of hemicellulose and the partial removal of lignin from the fibers Yue et al 2015). The aromatic C=C stretching in lignin in the spectra for KCF, OPMF, and EFBF appeared at the absorption bands 1614, 1619, and 1610 cm -1 , respectively.…”
Section: Fourier Transform Infrared Spectra Analysis Of Untreated Andmentioning
confidence: 93%
See 1 more Smart Citation
“…In addition, compared with the origin and NaOH treated fibers, B101.5s, B201.5s and B2010s exhibited lower TCI values, indicating a less crystalline structure and lower thermal stability (Yue et al, 2015). The phenomenon was caused by the strong destructive effect of NaClO 2 .…”
Section: Nomentioning
confidence: 90%
“…Because pyrolysis characteristics are highly correlated with the cellulose structure (Liu & Hu, 2008), the changed crystallinity and percentages of cellulose I/II hybrid fibers also contribute to define the thermal stability of the fibers. Yue et al (2015) reported that B2010 had a remarkable thermal stability, followed by B101.5; whereas B201.5 showed relatively lower decomposition temperatures. This trend was basically following the changing in crystallinity of these fibers (B101.5 > B2010 > B201.5).…”
Section: Nomentioning
confidence: 99%