Bioactivity behaviour of biodegradable material comprising bioactive glass

Abstract: International audienceBiocomposite of bioactive glass (BG) with chitosan polymer (CH) is prepared by freeze-drying technique. Obtained material is investigated by using several physico-chemical methods. The XRD and FTIR show the interface bonding interactions between glass and polymer. The specific surface and porosity of biocomposite were determined. In vitro assays were employed to evaluate the effect of chitosan addition on the glass by studying the chemical reactivity and bioactivity of the BG and BG/CH bi… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

0
21
0

Year Published

2013
2013
2020
2020

Publication Types

Select...
6

Relationship

1
5

Authors

Journals

citations
Cited by 20 publications
(21 citation statements)
references
References 21 publications
0
21
0
Order By: Relevance
“…However, hydroxyapatite (HA) phase has been formed after immersion of bioactive glass powder in the SBF for 2 days (Fig. 1b) [14] confirmed by appearance of two characteristic HA peaks at 26°(002) and 32°(211). Other less obvious peaks could also be seen at 40°(310), 46.7°( 222), 50°(213) and 53°(004).…”
Section: Characterisationmentioning
confidence: 89%
“…However, hydroxyapatite (HA) phase has been formed after immersion of bioactive glass powder in the SBF for 2 days (Fig. 1b) [14] confirmed by appearance of two characteristic HA peaks at 26°(002) and 32°(211). Other less obvious peaks could also be seen at 40°(310), 46.7°( 222), 50°(213) and 53°(004).…”
Section: Characterisationmentioning
confidence: 89%
“…The BG–CH composite containing 17 wt% of chitosan polymer was elaborated . First, CH polymer is a natural biodegradable polymer that is obtained by partial deacetylation of chitin, which is extracted from crustacean.…”
Section: Methodsmentioning
confidence: 99%
“…The BG-CH composite containing 17 wt% of chitosan polymer was elaborated. 20 First, CH polymer is a natural biodegradable polymer that is obtained by partial deacetylation of chitin, which is extracted from crustacean. CH with medium molecular weight of 480 000 Da and a degree of deacetylation of 85% was dissolved in a 1% acetic acid aqueous solution.…”
Section: Elaboration Of Bioactive Glass/chitosan Compositementioning
confidence: 99%
“…1b). [11,12] In detail, two well-defined characteristic peaks of HA at 2-θ values of 26  and 32  appeared. They correspond respectively to the (0 0 2) and (2 1 1) lattice planes in the structure of HA crystals.…”
Section: Characterizationmentioning