“…Due to the scaling process, after each iteration, lower frequencies are described. In other words, DWT analyses the EN signal using a pre-defined number of timescales by scaling and translation of wavelets [9,18,21,[23][24][25][26][27][28]. The energy present in those timescales could in turn be associated with the dominance of activation-or diffusion controlled processes, or processes under mixed control [7,9,16,18,21,[23][24][25][26][27][28][29][30].…”