Advanced atomic layer deposition (ALD): controlling the reaction kinetics and nucleation of metal thin films using electric-potential-assisted ALD

Abstract: Ru thin films are grown using electric potential assisted ALD (EA-ALD), modifying the thin film growth behavior with an electric potential applied to the substrate. The generated electric field increases...