A Novel Synthetic Nano-Catalyst (Ag2O3/Zeolite) for High Quality of Light Naphtha by Batch Oxidative Desulfurization Reactor

Abstract: Oxidative desulfurization process (ODS), enhanced with a novel metal oxide (Ag ions) as an active component over nano-zeolite that has not been reported in the literature, is used here to improve the fuel quality by removing mercaptan (as a model sulfur compound in the light naphtha). Nano-crystalline (nano-support (Nano-zeolite)) composite is prepared by Incipient Wetness Impregnation method loaded with a metal salt to obtain 0.5, 1 and 1.5% of Ag2O3 over Nano-zeolite. The new homemade nano-catalysts (Ag2O3/N… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1

Citation Types

0
1
0

Year Published

2022
2022
2024
2024

Publication Types

Select...
4
1

Relationship

0
5

Authors

Journals

citations
Cited by 5 publications
(1 citation statement)
references
References 40 publications
0
1
0
Order By: Relevance
“…Stannous chloride dihydrate (SnCl2.2H2O) has used as the metal precursor to preparation SnO2/rGO catalyst. The quantity of the active material of was added to deionized water and the solution was stirred for 60 minutes at room temperature till all Stannous chloride dihydrate dissolved in water [11,12]. Reduced graphene oxide has added to the prepared solution with continuous stirring of the mixture for 120 minutes at room temperature until the mixture is total impregnated.…”
Section: Preparation Of Sno2/rgo Composite Catalystmentioning
confidence: 99%
“…Stannous chloride dihydrate (SnCl2.2H2O) has used as the metal precursor to preparation SnO2/rGO catalyst. The quantity of the active material of was added to deionized water and the solution was stirred for 60 minutes at room temperature till all Stannous chloride dihydrate dissolved in water [11,12]. Reduced graphene oxide has added to the prepared solution with continuous stirring of the mixture for 120 minutes at room temperature until the mixture is total impregnated.…”
Section: Preparation Of Sno2/rgo Composite Catalystmentioning
confidence: 99%