“…Hence it is suggested to use precompacted powder pellets instead of loosely packed powder in a glass tube for assessing the wetting behaviour of submicrometer particles [11]. In order to eliminate the need for a reference liquid, the pore geometry factor f is calculated from the pore radius, r c , sample porosity, e, and sample radius, R as [11]:…”