“…Insulated iron powder (Fig. 1) offers several advantages over traditional steel in some applications, for example, the isotropic nature of the SMC combined with the unique shaping possibilities opens up for 3D-design solutions [55,56]. In recent years, effects of particle size, particle composition (Fe-Ni, Fe-Ni-Co, Fe-Si) [1][2][3][4][5][6][7][8], compaction parameters (warm compaction, pressure, lubricant), resin and wet chemical methods for creation of insulation layer around particles have been verified [2,6,7,53,60].…”