Propriedades Físicas da Madeira de Eucalyptus cloeziana F. Muell

Abstract: RESUMO Foram avaliadas propriedades físicas da madeira de 70 árvores da espécie Eucalyptus cloeziana com aproximadamente 10 anos de idade, provenientes de florestas localizadas na região centro-oeste do Estado de Minas Gerais. Foram determinados umidade, densidade básica e aparente e retratibilidade. As amostras apresentaram valores médios de 703 kg/m3, 843 kg/m3 e 916 kg/m3 para densidade básica, densidade aparente seca e densidade aparente a 12% de umidade, respectivamente. Quanto à retração radial, tangenci… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

0
4
1
1

Year Published

2019
2019
2024
2024

Publication Types

Select...
7

Relationship

0
7

Authors

Journals

citations
Cited by 7 publications
(6 citation statements)
references
References 20 publications
0
4
1
1
Order By: Relevance
“…Tangential and radial shrinkage of A. maripa and A. speciosa were around 5%. These results are opposite to those found in solid timber, in which the tangential shrinkage is significantly greater than the radial (Alves et al 2017;Lengowski et al 2021). However, palm trees do not present growth rings and radial cells as in wood, which is why, possibly, the same relationship was not found in tangential and radial shrinkage.…”
Section: Chemical and Physical Propertiescontrasting
confidence: 79%
“…Tangential and radial shrinkage of A. maripa and A. speciosa were around 5%. These results are opposite to those found in solid timber, in which the tangential shrinkage is significantly greater than the radial (Alves et al 2017;Lengowski et al 2021). However, palm trees do not present growth rings and radial cells as in wood, which is why, possibly, the same relationship was not found in tangential and radial shrinkage.…”
Section: Chemical and Physical Propertiescontrasting
confidence: 79%
“…The wood's basic density was determined according to Alves et al (2017). The wood's higher heating value (HHV) was determined according to ASTM D240-02 (2002), using dry grinded sifted material, with particle size between 40 and 60 mesh, in an adiabatic calorimeter.…”
Section: Methodsmentioning
confidence: 99%
“…For the eucalyptus firewood, the boiler's fuel, it was informed by the boiler operator the feed is about 1 cubic meter per hour of firewood. Being the standard cubic meter of 850 kg in accordance with Alves (2017), approximately, the fuel mass flow is 0.24 kg.s -1 , as described in Table 1.…”
Section: Exergoeconomic Analysis In a Food Industry Boiler: A Case Studymentioning
confidence: 99%