The 6061-T6 sheet and the DP 780 steel sheet were joined under the condition with the gap length d of 1.17 to 1.42 mm and discharge energy W of 3.0 kJ. The impact speed ranged from 430 to 460 m/s. The weld width showed a tendency to increase due to the increase of the collision speed. However, when the gap length exceeds 1.59 mm (impact speed of >460 m/s), the weld width became narrow. Considering that the electromagnetic force continues to apply on the flyer sheet after collides with the fixed sheet, it is desirable to perform the welding in a time shorter than the time t m when the collision time reaches the maximum current value. Therefore, the collision time is considered to be one of factors that affect the welding condition. As a result of experiments in consideration of above conditions, it was possible to achieve a strong lap joint of the 6061-T6 sheet and the DP 980 steel sheet, although the welding condition was limited as compared with the case of the DP 780 steel sheet. Thus, sound lap joint between 6061-T6 sheet and high-tensile steel sheet with 1 GPa class was achieved by magnetic pulse welding.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.