Alveolar bone loss has long been a challenge in clinical dental implant therapy. Simvastatin (SV) has been demonstrated to exert excellent anabolic effects on bone. However, the successful use of SV to increase bone formation in vivo largely depends on the local concentration of SV at the site of action, and there have been continuing efforts to develop an appropriate delivery system. Specifically, nanostructured lipid carrier (NLC) systems have become a popular type of encapsulation carrier system. Therefore, SV-loaded NLCs (SNs) (179.4 nm in diameter) were fabricated in this study, and the osteogenic effect of the SNs was evaluated in a critical-sized rabbit calvarial defect. Our results revealed that the SNs significantly enhanced bone formation in vivo, as evaluated by hematoxylin and eosin (HE) staining, immunohistochemistry, and a fluorescence analysis. Thus, this novel nanostructured carrier system could be a potential encapsulation carrier system for SV in bone regeneration applications.
Objectives. The present study intended to further verify that simvastatin-loaded nanomicelles (SVNs) enhanced the role of simvastatin (SV) in promoting osteoblast differentiation in vitro and to evaluate the effect of SVNs on bone defect repair in vivo. Methods. SVNs were synthesized by dialysis. MG63 cells were subjected to intervention with 0.25 μmol/l of SVNs and SV. A 3-(4,5-dimethylthiazol-2-yl)-5-(3-carboxymethoxyphenyl)-2-(4-sulfophenyl)-2H-tetrazolium (MTS) assay kit and flow cytometry were used to determine cell proliferation activity, cell cycle distribution, and apoptosis. The osteoblastic differentiation of MG 63 cells was evaluated by measuring alkaline phosphatase (ALP) activity, ALP staining, and the expression levels of the osterix (Osx) and osteocalcin (OC) proteins. In addition, 0.5 mg of SVNs or SV was applied to the skull defect area of rabbits. Micro-CT, hematoxylin and eosin (HE) staining, and Masson’s trichrome staining were used for qualitative and quantitative evaluation of new bone in three dimensions and two dimensions. Results. The SVNs had a mean diameter of 38.97 nm. The encapsulation and drug-loading efficiencies were 54.57 ± 3.15 % and 10.91 ± 0.63 % , respectively. In vitro, SVNs and SV can inhibit the proliferation activity and promote osteogenic differentiation of MG63 cells by arresting MG63 cells at the G0/G1 phase without increasing the apoptosis rate. In vivo quantitative results showed that the bone mineral density (BMD), bone volume (BV)/total volume (TV) ratio, and trabecular number (Tb.N) in the gelatin sponge with SVNs (SVNs-GS) group and gelatin sponge with SV (SV-GS) group were 362.1%, 292.0%; 181.3%, 158.0%; and 215.2%, 181.8% of those in the blank control (BC) group, respectively. Histological results identified the new bone tissue in each group as irregular fibrous bone, and the arrangement of trabecular bone was disordered. There were significantly more osteoblasts and new capillaries around the trabecular bone in the SVNs-GS group and SV-GS group than in both the BC and drug-free nanomicelle (DFNs) groups. Both in vitro and in vivo, SVNs exhibited greater osteogenic efficacy than SV. Conclusion. SVNs significantly improved the osteogenic efficacy of SV.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.
hi@scite.ai
10624 S. Eastern Ave., Ste. A-614
Henderson, NV 89052, USA
Copyright © 2024 scite LLC. All rights reserved.
Made with 💙 for researchers
Part of the Research Solutions Family.