Gold-palladium alloy plating was investigated in strongly agitated solutions containing 0.211M EDTA-2Na, 0.198M Na2SO3, 0.012M NaAsO2, 0.021M Au(SO3)23-and 0.024M Pd(en)23+ under condition crystal plane, and were fine grained and bright. Thus, gold-palladium alloy plating is advantageous as a substitute for expensive gold in the industry, and for noncyanide plating.
The anodic polarization behavior and time dependence of anodic current of 99.999% aluminum in 0.5M NaUl solution were examined. Pitting corrosion of super high purity aluminum in 0.5M NaCl at pH 8.5 is caused by Cl-which permeates cracks at the interface of the surface film and a rhombic corrosion product. This corrosion product mainly composed of Al, Fe and Si is formed at less noble potentials than the pitting potential.The pitting corrosion is affected by chemical dissolution in 0.5M NaCl solution at pH 10, and the pitting potential becomes noble. The limiting current in the anodic polarization curves is controled by diffusion of OH-in the solutions of pH 8.5 and 10. The corrosion potential of super high purity aluminum in 0.5M NaCI is about -0.76V at pH 4, -0.73V at pH 6, -0.72V at pH 8.5 and -0.72V at pH 10.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations鈥揷itations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.