We present, to the best of our knowledge, the first laser demonstration of an Yb-doped Gd(2)O(3) cubic crystal. This crystal was obtained by the flux method using an original borate-based solvent, which was particularly well suited to the growth of rare earth sesquioxide crystals at half the working temperature of classical growth techniques. This flux method is a very interesting alternative for the production of laser sesquioxide crystals, not only because it provides access to new matrices of the cubic polymorph, but also because it permits high Yb(3+)-doping levels for these crystals. The first laser results of two highly Yb(3+)-doped sesquioxides, namely Gd(2)O(3) and Y(2)O(3), grown by this flux method are presented here, including the Ti:sapphire and diode pumping configurations. Laser efficiencies and emission spectra for these two crystals were studied and compared.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.