The objective of this research was to evaluate the performance of metal-plate-connected truss joints subjected to cyclic loading conditions that simulated seismic events in the lives of the joints. We also investigated the duration of load factor for these joints. We tested tension splice joints and heel joints from a standard 9.2-m Fink truss constructed from 38-× 89-mm Douglas-fir lumber: 10 tension splice joints for static condition and for each of 6 cyclic loading conditions (70 joints total) and 10 heel joints for static condition and for each of 3 cyclic loading conditions (40 joints total). We evaluated results by comparing the strengths of the control group (static) with those of the cyclic loading groups. None of the cyclic loading conditions showed any strength degradation; however, there was significant stiffness degradation for both types of joint. The results of this research show that the current duration of load factor of 1.6 for earthquake loading is adequate for these joints.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.
customersupport@researchsolutions.com
10624 S. Eastern Ave., Ste. A-614
Henderson, NV 89052, USA
Copyright © 2024 scite LLC. All rights reserved.
Made with 💙 for researchers
Part of the Research Solutions Family.