Objective: The aim of this study was to evaluate the effect of sealants on the prevention of enamel demineralization and on biofilm metabolic activity. Materials and Methods: Cavity preparations were performed on 45 blocks of bovine teeth (4x4x4 mm) randomly assigned to three groups (n=15): RI-Riva Light Cure®/SDI; EM-Embrace™ WetBond™ Pulpdent Corp.®; and CO-Natural Flow/DFL resin (negative control). The sealed blocks were subjected to thermocycling (500 cycles/30 s). Half of the blocks were covered with acidresistant varnish to create a control area (RI, EM, and CO) and an experimental area (RI-EX, EM-EX, and CO-EX). They were subsequently exposed to Streptococcus mutans biofilm for assessment of demineralization by the Knoop microhardness test (50 g/15 s), at 25, 50, 100, 150, and 200 μm from the interface. In another test, the cylinders of the sealants (4 mmx3 mm) were subjected to the biofilm metabolic activity test. Results: The RI-EX group showed higher microhardness than CO-EX (p<0.05) and less demineralization when compared to RI at all distances. Microbial activity was lower in EM compared to CO, but not statistically significant in relation to RI. Conclusion: Both sealants can inhibit enamel demineralization in the presence of S. mutans biofilm.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.