In this paper, high-quality single crystals of (Mo0.85Nb0.15)Si2, around 8 mm in diameter and 90 mm in length, have been grown by optical heating floating zone method. Effects of chemical composition and growth rate on forming C40 structured single crystal were studied. Aligned C40/C11b lamellar structured can be formed in the as-grown crystals after post annealing at temperatures between 1473 and 1873 K. Chemical composition as well as annealing temperature are found to be two important factors to form C11b lamellae in the C40 matrix. Fully C40/C11b lamellar structure was formed after annealing at 1873 K in the present work. The aligned C40 and C11b lamellae follow a crystallographic orientation relationship of (0001)C40//(110)C11b. Dislocations were observed in some coarse C11b lamellae but never in C40 lamellae of the duplex structure. This is probably due to accumulation of misfit strain during formation of C40/C11b lamellae.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.