Steel production and processing are connected with high temperatures. Due to a reaction between hot surface of the steel and oxygen contained in surrounding atmosphere, oxides are formed on the surface of the steel. Created layer of oxides is called scales and has influence on cooling and quality of steel. Thickness and structure of scale layer are influenced by chemical composition of the steel, temperature and atmosphere during oxidation. Scale layer can be considerably porous which has a significant influence on thermal conductivity of this layer, because air pores have much lower thermal conductivity compared to scales. Steel samples were prepared and porosity of scale layer was studied. Further, the average thermal conductivity of porous scale layer was determined for different regimes of oxidation by FEM modelling. It was found that the average thermal conductivity of porous scale layer is influenced not only by porosity of scale layer, but also by distribution of air pores, which can has a significant effect.
Steel production and processing are connected with the formation of an oxide layer on a hot surface of steel. The oxide layer influences cooling and the final quality of the steel. Spray cooling is mainly influenced by water impingement density and by surface temperature, but the influence of the oxide layer is not negligible. The oxide layer can be considerably porous. The porosity of the oxide layer significantly influences its thermal conductivity, because air pores have much lower thermal conductivity compared to pure oxides. In this paper, the influence of the oxide layer on water spray cooling is experimentally and numerically investigated. The heat transfer coefficient of an oxidized steel surface and a clean steel surface are compared and the effect of the oxide layer on the Leidenfrost temperature is studied. Also, the porosity of the oxide layer and the average thermal conductivity of the porous oxide layer are determined for different oxidation regimes.
Hydraulic descaling is an inherent part of the hot rolling process but can sometimes also be applied in the heat treatment process, continuous casting and other processes. The need for optimal descaling is linked with the quality of the final product. The goal is usually simplified to the complete removal of the scale layer from the hot surface. The descaled surfaces are often wide and a number of nozzles must be used. The quality problems are almost exclusively connected with the overlap of water jets. An experimental study of overlap optimization is presented in this paper. A new approach using in-line configuration of jets is introduced and discussed. This paper also describes why even the completely oxide-free surface achieved after descaling the unit can be a far from optimal solution. Thermal strips on the hot surface cause much more intensive oxidation of the hot part and much slower oxidation in the cold strips on the descaled surface. The speed of oxide formation on the steel surface is exponentially dependent on the surface temperature. Temperature nonhomogeneity after descaling in the rolling process can cause the same defects on the surface of the final product as poor descaling. Temperature aspects with links to heat loss and secondary oxidation are discussed.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.
hi@scite.ai
10624 S. Eastern Ave., Ste. A-614
Henderson, NV 89052, USA
Copyright © 2024 scite LLC. All rights reserved.
Made with 💙 for researchers
Part of the Research Solutions Family.