Mesoporous ZnO films composed of interconnected porous nanoplates were prepared by an electrochemical deposition-pyrolytic conversion approach and constructed into the photoanodes of dyesensitized solar cells (DSSCs). Precursor nanoplates grown on conducting glass substrates were transformed into ZnO porous nanoplates by calcination at 400 °C for 1 h. Correlations between the ZnO film thickness and the electrochemical deposition time were determined in order to prepare ZnO films of various thicknesses and to study the effect of the film thickness on the photovoltaic performance of DSSCs. The optimal film thickness was determined to be approximately 27 μm, and the best performing cell reached an energy conversion efficiency of 2.91%. The results show that the ZnO porous nanoplate network so prepared is suitable for DSSC applications.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.