The aim of the study was to experimentally determine the effect of the heat treatment parameters of anthracites from Donetsk basin on the properties of carbon materials when using shock heating, typical of furnaces with a fluidized electrothermal bed. Anthracite was treated in an electric thermal furnace at the heating rate of 1000 K/min and the holding time of 10–20 min. The processing temperature range was 1500–30000С. For processing, we used initial anthracites and anthracites after calcination at 1100–12000С. The properties of the carbon material were investigated by X-ray radiographic analysis, XRF analysis and diffuse reflectance infrared Fourier transform. It was found that pre-calcination did not produce any effect on the properties of anthracite carbon materials during shock heating and holding time less than 1 hour. Based on the results of studies of anthracite heat treatment while changing the holding time, the following kinetic characteristics of transformations during shock heating were determined: the preexponential coefficient of 1.79 and the apparent activation energy of 103.85 kJ/mol. Thermal processing of anthracite from Donetsk coal basin in electric furnaces with the fluidized bed at the temperature 30000С for 55–60 min allows obtaining the crystalline structure characteristic of artificial graphite with necessary electroconductivity and element composition.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.