KEYWORDSMulti-walled carbon nanotubes; Toughened adhesives; Fracture energy; Cohesive zone model; Double cantilever beam.Abstract. In this paper, the in uence of the outer diameter of multi-walled carbon nanotubes (MWCNTs) on the fracture behavior of epoxy adhesives was investigated experimentally and numerically. MWCNTs with three di erent outer diameters of less than 8, 20-30, and 50-80 nm were used to toughen the epoxy adhesive. Double Cantilever Beam specimens were tested to determine the fracture energy. The results indicated that improvement in the adhesive fracture resistance by introducing MWCNTs was considerably dependent on the outer diameter of MWCNTs. Toughening the epoxy adhesive by incorporating MWCNTs with 8 nm diameter improved the adhesive fracture energy three times higher compared to the MWCNTs with larger diameters. The SEM fractography of the fracture surfaces was also utilized to assess the governing fracture mechanisms occurred in the toughened epoxy adhesives. Moreover, a cohesive zone model was used for numerical investigation of the e ect of the MWCNT diameter on the damage behavior of epoxy adhesives.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.