BackgroundThe purpose of this study was to compare the shear bond strength and adhesive remnant index (ARI) at the enamel-bonding interface of precoated and conventionally bonded brackets, utilizing standardized procedures.MethodsThe test sample consisted of 90 recently extracted bovine permanent mandibular incisors. The teeth were bonded using the same protocol and were tested in three different situations. A material testing systems machine was utilized for debonding, and the remaining adhesive on the tooth was recorded.ResultsImmediately after bonding, we found that the shear bond strength of the precoated brackets (6.27 MPa) was significantly higher than that of conventional brackets (5.37 MPa) (p < 0.05). However, no significant differences in bond strength were found between the two bracket systems after 24 h of bonding or after thermocycling. The conventional brackets had higher ARI scores than the precoated bracket systems immediately after bonding and after 24 h.ConclusionsSince there were no significant differences in the bonding strength after 24 h, the immediate bonding strength of the precoated brackets during the first day does not appear to be a major advantage over the conventional bracket systems. However, less adhesive on the tooth after debonding is an advantage of precoated brackets.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.