Using neutron diffraction we determined internal residual stress in the stainless steel AISI 310S carrier tape with a thickness of 100 μm and a width of 4 mm after mechanical polishing and the ABAD deposition of the textured YSZ buffer layer. It is shown that mechanical polishing causes a slight distension of the tape in the rolling plane. After the deposition of the YSZ layer, uniform tensile stress of 70 MPa isotropic in the rolling plane was observed inside the tape. Calculations have shown that it results from relaxation of compressive stress acting on the surface of the tape in a layer several times thicker than the YSZ layer. It is assumed that the surface of the tape is plastically deformed during the YSZ deposition. Keywords: residual stress, YSZ buffer layer, HTS-2G wire, AISI 310S carrier tape, neutron stress diffractometry.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.