This work investigates the correlation between the in-vitro wear resistance and the nanomechanical properties of dental sealants commercially available. Mechanical properties, namely hardness (H) and elastic modulus (E), were assessed by nanoindentation technique. The coated samples presented lower H and E values than the Z250 composite resin substrate. Such measurements were used to calculate H/E ratios. Wear tests were carried out in water by using a pin-on-plate apparatus. Scars formed on the samples were qualitatively examined by optical microscopy, while their wear depths were measured by contact profilometry. Based on the findings, an empirical correlation between the wear depths and H/E was obtained. A high H/E ratio was associated to surfaces with enhanced wear resistance. For the tribological conditions here employed, the H/E ratio could be, therefore, considered a useful parameter for ranking the in-vitro wear of dental sealants.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.