Calcium phosphates (Ca-P) are used commonly as artificial bone substitutes to control the biodegradation rate of an implant in the body fluid. This study examined the in vitro proliferation of human bone marrow-derived mesenchymal stem cells (hBMSCs) on triphasic Ca-P samples. For this aspect, hydroxyapatite (HA), dicalcium phosphate dehydrate (DCPD), and calcium hydroxide (Ca(OH) ) were mixed at various ratios, cold compacted, and sintered at 1250°C in air. X-ray diffraction showed that the β-tricalcium phosphate (TCP) to α-TCP phase transformation increased with increasing DCPD/HA ratio. The micro-hardness deceased with increasing TCP content, whereas the mean grain size and porosity increased with increasing TCP concentration. To evaluate the in vitro degree of adhesion and proliferation on the HA/TCP samples, human BMSCs were incubated on the HA/TCP samples and analyzed by a cells proliferation assay, expression of the extracellular matrix (ECM) genes, such as α-smooth muscle actin (α-SMA) and fibronectin (FN), and FITC-phalloidin fluorescent staining. In terms of the interactions of human BMSCs with the triphasic Ca-P samples, H50T50 (Ca/P = 1.59) markedly enhanced cell spreading, proliferation, FN, and α-SMA compared with H100T0 (Ca/P = 1.67). Interestingly, these results show that among the five HA/TCP samples, H50T50 is the optimal Ca-P composition for in vitro cell proliferation. © 2015 Wiley Periodicals, Inc. J Biomed Mater Res Part B: Appl Biomater, 105B: 72-80, 2017.
Ca-P and silicon based materials have become very popular as bone tissue engineering materials. In this study, water-glass (also known as sodium silicate glass) was coated on sintered hydroxyapatite (HA) and HA-TCP (TCP stands for tricalcium phosphate) samples and subsequently heat-treated at 600°C for 2 hrs. X-rays diffraction showed the presence of β- and α-TCP phases along with HA in the HA-TCP samples. Samples without coating, with water-glass coating, and heat-treated after water-glass coating were used to observe the adhesion and proliferation response of bone marrow derived-mesenchymal stem cells (MSCs). Cell culture was carried out for 4 hrs, 1 day, and 7 days. Interestingly, all samples showed similar response for cell adhesion and proliferation up to 7-day culture but fibronectin, E-cadherin, and osteogenic differentiation related genes (osteocalcin and osteopontin) were significantly induced in heat-treated water-glass coated HA-TCP samples. A water-glass coating on Ca-P samples was not found to influence the cell proliferation response significantly but activated some extracellular matrix genes and induced osteogenic differentiation in the MSCs.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.
hi@scite.ai
10624 S. Eastern Ave., Ste. A-614
Henderson, NV 89052, USA
Copyright © 2024 scite LLC. All rights reserved.
Made with 💙 for researchers
Part of the Research Solutions Family.