Alloy 22 (N06022) may be susceptible to crevice corrosion in chloride solutions. Nitrate acts as an inhibitor to crevice corrosion. Several papers have been published regarding the effect of nitrate on the corrosion resistance of Alloy 22 at temperatures 100°C and lower. However, very little is known about the behavior of this alloy in highly concentrated brines at temperatures above 100°C. In the current work, electrochemical tests have been carried out to explore the anodic behavior of Alloy 22 in high chloride high nitrate electrolytes at temperatures as high as 160°C at ambient atmospheres. Even though Alloy 22 may adopt corrosion potentials in the order of + O S V (in the saturated silver chloride scale), it does not suffer crevice corrosion if there is high nitrate in the solution. That is, the inhibitive effect of nitrate on crevice corrosion is active for temperatures higher than 100°C.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.
hi@scite.ai
10624 S. Eastern Ave., Ste. A-614
Henderson, NV 89052, USA
Copyright © 2024 scite LLC. All rights reserved.
Made with 💙 for researchers
Part of the Research Solutions Family.