The aim of this study was to determine the non-intentionally added substances--formaldehyde and trace metals--at 4% acetic acid conditions in rubber and metallic packaging/utensils. The temperature effect on migration in rubber and metallic packaging/utensils was monitored at 60 °C and 100 °C under acidic (pH< 3) circumstances. The concentrations were: formaldehyde--23.1 μg kg⁻¹, lead--13.41 μg kg⁻¹, cadmium--0.15 μg kg⁻¹, total arsenic--2.02 μg kg⁻¹ and nickel--2.92 μg kg⁻¹ at 60 °C and formaldehyde--148.9 μg kg⁻¹, lead--17.04 μg kg⁻¹, cadmium--0.14 μg kg⁻¹, total arsenic--7.25 μg kg⁻¹ and nickel--8.7 μg kg⁻¹ at 100 °C. A significant difference was noticed in formaldehyde and total arsenic between both temperatures (p < 0.01), which was not present in other trace metals. In conclusion, formaldehyde and total arsenic were more sensitive with cooking temperature than the other metals.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.