PET-poly (ethylene terephthalate)-bottle surfaces were exposed to chemical agents and evaluated with middle infrared spectroscopy (MIR) and near infrared hyperspectral imaging (HSI-NIR). Images (928-2.524 nm) were acquired at different times from bottle surfaces exposed to alkaline, acidic and ethanolic media. Savitzky-Golay smoothing (2 nd order polynomial and 5-point window) combined with Standard Normal Variate (SNV) was used for pre-processing data. Scores from principal component analysis (PCA) on images showed discrimination of PET according to exposure time, particularly when employing NaOH. After the first two hours of chemical exposure, significant contribution of the (-CO + OH) combination band indicated formation of glycol ethylene on the PET surface, which was confirmed from PCA loading plots. MIR reflectance spectra ranged from 4.000 to 650 cm-1. Changes in spectral intensities could be associated with depolymerization of PET when exposed to NaOH. These were confirmed with PCA and attributed to the carboxylate group of terephthalate.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.