1991
DOI: 10.1021/la00054a029
|View full text |Cite
|
Sign up to set email alerts
|

Use of electroactive thiols to study the formation and exchange of alkanethiol monolayers on gold

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

21
225
0

Year Published

2000
2000
2011
2011

Publication Types

Select...
6
3

Relationship

0
9

Authors

Journals

citations
Cited by 271 publications
(246 citation statements)
references
References 0 publications
21
225
0
Order By: Relevance
“…The resulting surface coverage was calculated from the area under the voltammetric peak as the scan rate is varied in the range 0.1-2 V s -1 , and was found to be 4.64 × 10 -11 mol/cm 2 . This value is about one order of magnitude smaller than those reported in literature for alkanethiol SAMs on Au(111) [72][73][74]. However, it is not surprising, since the steric hindrance It is interesting to note that the peak separation E p is greater than 0 and slightly increases with increasing scan rates (50 mV at 1 V/s as compared to 30 mV at 100 mV/s).…”
Section: Photophysical Characterization In Solutionmentioning
confidence: 56%
“…The resulting surface coverage was calculated from the area under the voltammetric peak as the scan rate is varied in the range 0.1-2 V s -1 , and was found to be 4.64 × 10 -11 mol/cm 2 . This value is about one order of magnitude smaller than those reported in literature for alkanethiol SAMs on Au(111) [72][73][74]. However, it is not surprising, since the steric hindrance It is interesting to note that the peak separation E p is greater than 0 and slightly increases with increasing scan rates (50 mV at 1 V/s as compared to 30 mV at 100 mV/s).…”
Section: Photophysical Characterization In Solutionmentioning
confidence: 56%
“…• C for 2 h only, in order to limit the exchange between thiol species as detailed elsewhere [18,19].…”
Section: Fabrication Of Nanopatterned Gold Surfacesmentioning
confidence: 99%
“…10 The voltammograms shown in Figure 2a reveal a trend towards an increasing faradaic current for Ru(NH 3 ) 6 Cl 3 reduction over time through β-CD-induced pores in the SAM. Since the SAM formed for 10 minutes in a pure nhexadecanethiol solution yields a largely passive electrode for electron transfer (see Figure 1c), we believe that the initial contact of the gold surface with the β-CD/n-hexadecanethiol mixed solution results in a high surface concentration of n-hexadecanethiol, which is being replaced slowly by thiolated β-CD as time goes on.…”
Section: Resultsmentioning
confidence: 96%
“…2, [8][9][10] The dynamic nature of the equilibrium has been demonstrated by exchange reactions such as the exchange of n-alkanethiols with ferrocene-labeled alkanethiols 8 and self-exchange of isotopically labeled compounds. 10 The voltammograms shown in Figure 2a reveal a trend towards an increasing faradaic current for Ru(NH 3 ) 6 Cl 3 reduction over time through β-CD-induced pores in the SAM.…”
Section: Resultsmentioning
confidence: 99%