Unusually tight aggregation in detonation nanodiamond: Identification and disintegration

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1
1
1

Citation Types

10
442
1
6

Year Published

2008
2008
2018
2018

Publication Types

Select...
5
4

Relationship

0
9

Authors

Journals

citations
Cited by 585 publications
(459 citation statements)
references
References 12 publications
10
442
1
6
Order By: Relevance
“…They were also characterized by FTIR studies [7][8]. At 1073 K, the carbon / oxygen bonds underwent weak modifications (figure 1b) while they are strongly removed after the annealing at 1173 K (figure 1c).…”
Section: Discussionmentioning
confidence: 99%
See 1 more Smart Citation
“…They were also characterized by FTIR studies [7][8]. At 1073 K, the carbon / oxygen bonds underwent weak modifications (figure 1b) while they are strongly removed after the annealing at 1173 K (figure 1c).…”
Section: Discussionmentioning
confidence: 99%
“…Moreover, previous Fourier Transform Infrared (FTIR) spectra underlined that UDD termination involves the presence of hydroxyls (C-OH), ether (C-O-C) and carbonyls (C=O) groups [7][8] resulting from the severe acid treatment applied prior the dispersion of diamond nanoparticles in water. 1 2 3 4 5 6 7 8 9 10 11 12 13 14 15 16 17 18 19 20 21 22 23 24 25 26 27 28 29 30 31 32 33 34 35 36 37 38 39 40 41 42 43 44 45 46 47 48 49 50 51 52 53 54 55 56 57 The morphology of the nanoseeded surface is depicted on the figure 2.…”
Section: Initial Si(100) Nanoseeded Surfacementioning
confidence: 99%
“…Each scaffold contained 1 µg of BMP-2. Acid purifi ed detonation diamond (Gansu Lingyun Corp., Lanzhou, China) was subjected to attrition milling using a method previously described [ 27 ] achieving a narrow size distribution at ≈5 nm particle diameter (measured by dynamic light scattering in water) and very low agglomeration of the diamond particles. Scaffolds were modifi ed with the nDP solution (2 wt%, i.e., 20 mg mL −1 ) by a vacuum technique: 0.5 mL nDP solution and one scaffold were put in a glass beaker and perfused in vacuum (Oerlikon Leybold, TRIVAC D 65B).…”
Section: Colloidal Ndp Production and Scaffolds Modifi Ed With Ndp Plmentioning
confidence: 99%
“…2 A nanodiamond with a mixed composition of surface groups can be oxidised and terminated with oxygencontaining functional groups or reduced to produce a homogeneous hydrogen surface termination bead milling and sonication (Krüger et al 2005;Fu et al 2007;Faklaris et al 2008). Through a combination of these techniques we were first able to observe NV centres in isolated 5-nm nanodiamonds (Bradac et al 2010).…”
Section: Oxidation/carboxylation Reductionmentioning
confidence: 99%