Unusual cold rolled texture in an Mg-2.0Zn-0.8Gd sheet

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
4
1

Citation Types

0
10
0

Year Published

2017
2017
2024
2024

Publication Types

Select...
10

Relationship

2
8

Authors

Journals

citations
Cited by 69 publications
(10 citation statements)
references
References 34 publications
0
10
0
Order By: Relevance
“…The LAGBs resulted from the accumulation of dislocations and/or the formation of sub-grain boundaries in the deformed microstructure. With the strain increases, the LAGBs transformed into HAGBs by absorbing the mobile dislocations, eventually modifying the sub-grains into new DRXed grains [ 36 , 37 ]. It was also found that continuous dynamic recrystallization (CDRX) occurred in the RBE process.…”
Section: Resultsmentioning
confidence: 99%
“…The LAGBs resulted from the accumulation of dislocations and/or the formation of sub-grain boundaries in the deformed microstructure. With the strain increases, the LAGBs transformed into HAGBs by absorbing the mobile dislocations, eventually modifying the sub-grains into new DRXed grains [ 36 , 37 ]. It was also found that continuous dynamic recrystallization (CDRX) occurred in the RBE process.…”
Section: Resultsmentioning
confidence: 99%
“…As the cumulative strain increases, these LAGBs can be transformed into HAGBs by trapping more moving dislocations. Eventually, new DRXed grains (marked as blue arrows) are obtained [ 40 , 41 ] and expressed as a sudden rise in the point-to-point curve in Figure 13 f. This is a typical continuous dynamic recrystallization (CDRX) mechanism [ 28 , 42 ]. In addition, it can be observed from Figure 13 d that the grain boundaries of the coarse grains G2 are serrated (marked as purple arrows), and the sub-grains are separated from the coarse grains through the sub-grain boundaries, and new DRXed grains are formed along the serrated grain boundaries, which is a typical discontinuous dynamic recrystallization (DDRX) mechanism [ 43 ].…”
Section: Resultsmentioning
confidence: 99%
“…However, some DRXed grains also formed along the LABs, marked by the white arrows (Figure 6a). Usually, LAGBs result from the accumulation of dislocations and formation of sub-GBs in the large grains [33,34]. With the increasing strain, these LAGBs trapped more mobile dislocations and transformed themselves into HAGBs, ultimately turning sub-grains into DRXed grains, which indicated the operation of CDRX.…”
Section: Resultsmentioning