2015
DOI: 10.1016/j.matdes.2014.08.068
|View full text |Cite
|
Sign up to set email alerts
|

Tyranno SA3 fiber–ZrB2 composites. Part I: Microstructure and densification

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1
1

Citation Types

1
26
0

Year Published

2015
2015
2022
2022

Publication Types

Select...
4
2

Relationship

1
5

Authors

Journals

citations
Cited by 29 publications
(31 citation statements)
references
References 18 publications
(46 reference statements)
1
26
0
Order By: Relevance
“…Pressureless sintering of TaC-MoSi 2 system generally requires a temperature around 1950°C [11], but in this case it was set at 2100°C for 3 h in order to let the b ? a SiC polytypic transformation to completely occur.…”
Section: Reinforced Materialsmentioning
confidence: 99%
See 4 more Smart Citations
“…Pressureless sintering of TaC-MoSi 2 system generally requires a temperature around 1950°C [11], but in this case it was set at 2100°C for 3 h in order to let the b ? a SiC polytypic transformation to completely occur.…”
Section: Reinforced Materialsmentioning
confidence: 99%
“…a SiC polytypic transformation. MoSi 2 was selected as sintering aid in view of its role in favoring the densification through formation of transient liquid phases and of its refractoriness at high temperature [5,11]. Little amount of liquid phases formed at 2010°C, owing to the eutectic between MoSi 2 and SiC [16], certainly helped the local rearrangement and agglomeration of SiC rounded particles and favored their evolution to platelets leaving clean grain boundaries with the matrix.…”
Section: Sic Plateletsmentioning
confidence: 99%
See 3 more Smart Citations