Advanced Solid State Lasers 1998
DOI: 10.1364/assl.1998.fc15
|View full text |Cite
|
Sign up to set email alerts
|

Tunable Output Around 8μm from a Single Step AgGaS2 OPO Pumped at 1.064μm

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1

Citation Types

0
4
0

Year Published

2012
2012
2023
2023

Publication Types

Select...
5

Relationship

0
5

Authors

Journals

citations
Cited by 5 publications
(4 citation statements)
references
References 3 publications
0
4
0
Order By: Relevance
“…The samples showed a damage threshold of about 83 MW/cm 2 (1064 nm, 5 ns). This value is higher than that of AgGaS 2 (AGS), and the latter is a commercially used IR NLO crystal with the LDT at about 30 MW/cm 2 …”
Section: Resultsmentioning
confidence: 89%
“…The samples showed a damage threshold of about 83 MW/cm 2 (1064 nm, 5 ns). This value is higher than that of AgGaS 2 (AGS), and the latter is a commercially used IR NLO crystal with the LDT at about 30 MW/cm 2 …”
Section: Resultsmentioning
confidence: 89%
“…The samples showed a damage threshold of about 190 MW/cm 2 (1064 nm, 5 ns). This value is much higher than that of AgGaS 2 (AGS), and the latter is a commercially used IR NLO crystal with the LDT at about 30 MW/cm 2 …”
Section: Resultsmentioning
confidence: 91%
“…In addition, the LDT measurements of MSP indicate that MSP exhibits a relatively high LDT of 70 MW/cm 2 , exceeding 2 times that of the benchmark AGS (30 MW/cm 2 ) …”
Section: Results and Discussionmentioning