The stress corrosion cracking (SCC) characteristics of Zircaloy-2 sheets in methanol-0.4 vol. pct. hydrochloric acid have been studied in the annealed and cold-rolled conditions using longitudinal and transverse specimens. The times to failure for annealed longitudinal specimens were longer than those for similarly tested transverse specimens at stress levels below -45% UTS. The cold-rolled specimens developed resistance to SCC, but failed totally by cleavage when notched, unlike annealed specimens which failed by intergranular initiation followed by cleavage. The crystallographic texture developed by cold rolling is such that the crack initiation is difficult because of quicker passivation characteristics of the crack initiating plane. The texture also gives unfavourable orientation of slip and twinning planes with respect to tensile axis. The crack initiating planes are identified with the help of X-ray pole figures. The apparent activation energy is found to be texture dependent at a given stress level. On the basis of apparent activation energy measurements, dynamic tests at constant cross-head speeds and electrochemical measurements, the mechanism of SCC is identified to be the one involving stress-aided anodic dissolution.Die Spannungsriakorrosion von Zircaloy-2-Blech wurde unter Verwendung von gegliihten und kaltgewalzten, in Langs-und Querrichtung ausgeglichenen Proben in 0,4 Vo1.-% methanolischer Salzsaurelosung untersucht. Die Zeit bis zur RiRbildung war bei den Langsproben langer als bei Querproben unter sonst gleichen Bedingungen (Belastung unter 45% der Zugfestigkeit). Die kaltgewalzten Proben waren zwar gegen SpannungsriRkorrosion bestandig, erlitten jedoch Spaltbruch, wenn sie gekerbt wurden, wahrend die gegliihten Proben ein anfangliches interkristallines RiRstadium mit anschlieflendem Spaltbruch zeigten. Durch das Kaltwalzen wird eine Kristalltextur gebildet, welche die ReiBeinleitung erschwert, da die riRauslosenden Ebenen sich rasch passivieren. Diese Textur enthalt auch Gleit-und Zwillingsebenen mit gegeniiber der Zugachse ungiinstiger Orientierung. Die riaauslosenden Ebenen werden mit Hilfe der Rontgen-Polfiguren identifiziert. Die scheinbare Aktivierungsenergie ist bei gegebener Belastung texturabhangig. Aufgrund der gemessenen scheinbaren Aktivierungsenergie, der dynamischen Untersuchungen mit konstanter Dehnung und der elektrochemischen Messungen wird der Mechanismus der Spannungsriakorrosion als durch Belastung geforderte anodische Auflosung identifiziert.
The stress corrosion cracking (SCC) characteristics of Zircaloy-2 sheets in methanol-0.4 vol. pct. hydrochloric acid have been studied in the annealed and cold-rolled conditions using longitudinal and transverse specimens. The times to failure for annealed longitudinal specimens were longer than those for similarly tested transverse specimens at stress levels below -45% UTS. The cold-rolled specimens developed resistance to SCC, but failed totally by cleavage when notched, unlike annealed specimens which failed by intergranular initiation followed by cleavage. The crystallographic texture developed by cold rolling is such that the crack initiation is difficult because of quicker passivation characteristics of the crack initiating plane. The texture also gives unfavourable orientation of slip and twinning planes with respect to tensile axis. The crack initiating planes are identified with the help of X-ray pole figures. The apparent activation energy is found to be texture dependent at a given stress level. On the basis of apparent activation energy measurements, dynamic tests at constant cross-head speeds and electrochemical measurements, the mechanism of SCC is identified to be the one involving stress-aided anodic dissolution.Die Spannungsriakorrosion von Zircaloy-2-Blech wurde unter Verwendung von gegliihten und kaltgewalzten, in Langs-und Querrichtung ausgeglichenen Proben in 0,4 Vo1.-% methanolischer Salzsaurelosung untersucht. Die Zeit bis zur RiRbildung war bei den Langsproben langer als bei Querproben unter sonst gleichen Bedingungen (Belastung unter 45% der Zugfestigkeit). Die kaltgewalzten Proben waren zwar gegen SpannungsriRkorrosion bestandig, erlitten jedoch Spaltbruch, wenn sie gekerbt wurden, wahrend die gegliihten Proben ein anfangliches interkristallines RiRstadium mit anschlieflendem Spaltbruch zeigten. Durch das Kaltwalzen wird eine Kristalltextur gebildet, welche die ReiBeinleitung erschwert, da die riRauslosenden Ebenen sich rasch passivieren. Diese Textur enthalt auch Gleit-und Zwillingsebenen mit gegeniiber der Zugachse ungiinstiger Orientierung. Die riaauslosenden Ebenen werden mit Hilfe der Rontgen-Polfiguren identifiziert. Die scheinbare Aktivierungsenergie ist bei gegebener Belastung texturabhangig. Aufgrund der gemessenen scheinbaren Aktivierungsenergie, der dynamischen Untersuchungen mit konstanter Dehnung und der elektrochemischen Messungen wird der Mechanismus der Spannungsriakorrosion als durch Belastung geforderte anodische Auflosung identifiziert.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.
customersupport@researchsolutions.com
10624 S. Eastern Ave., Ste. A-614
Henderson, NV 89052, USA
Copyright © 2024 scite LLC. All rights reserved.
Made with 💙 for researchers
Part of the Research Solutions Family.