Thermophysical properties of cross-linked polyethylene during thermal aging

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1
1
1

Citation Types

0
2
0

Year Published

2023
2023
2024
2024

Publication Types

Select...
6
2

Relationship

0
8

Authors

Journals

citations
Cited by 9 publications
(6 citation statements)
references
References 21 publications
0
2
0
Order By: Relevance
“…Figure 3d contains the melting range of each sample. Generally, the melting range of polymer is closely correlated with its lattice perfection, the more perfect lattice almost correspond to the narrower melting range 29 . After 2 h of heat aging, due to the high temperature may lead to crystals destruction, the melting range of both FDY and UVFDY became wider (28.4 ± 0.3 and 25.1 ± 0.4°C, respectively).…”
Section: Resultsmentioning
confidence: 98%
See 1 more Smart Citation
“…Figure 3d contains the melting range of each sample. Generally, the melting range of polymer is closely correlated with its lattice perfection, the more perfect lattice almost correspond to the narrower melting range 29 . After 2 h of heat aging, due to the high temperature may lead to crystals destruction, the melting range of both FDY and UVFDY became wider (28.4 ± 0.3 and 25.1 ± 0.4°C, respectively).…”
Section: Resultsmentioning
confidence: 98%
“…Generally, the melting range of polymer is closely correlated with its lattice perfection, the more perfect lattice almost correspond to the narrower melting range. 29 After 2 h of heat aging, due to the high temperature may lead to crystals destruction, the melting range of both FDY and UVFDY became wider (28.4 ± 0.3 and 25.1 ± 0.4 C, respectively). However, when the aging time exceeded 2 h, the melting range of UVFDY became wider while that of FDY became narrower, demonstrating that the crosslinked network of UVFDY may lead it difficult to form regular lattice during heat aging.…”
Section: Dsc Analysismentioning
confidence: 96%
“…The recycled is XLPE foam was used as the core component of the hybrid material. 31,32 The closed-cell structure of XLPE foam traps air inside the material, giving it outstanding thermal insulation capabilities. 33 Its poor heat conductivity means that less heat will move through the material.…”
Section: Methodsmentioning
confidence: 99%
“…Xing等 [21] 将茂金属聚乙烯(metallocene polyethylene, MPE)作 为 成 核 剂 与 XLPE共 混 , 材料共混后的晶体结构更致密, 分子间相互作用更 强, 而材料内部自由体积的减小和载流子平均自由 程的缩短, 可以减弱高能电子对分子链的损伤, 从 而抑制电树枝退化过程. Zhao等 [22] [19] . 联的过程, 如图3(a)所示 [24] .…”
Section: 然而 Xlpe电缆绝缘材料在复杂的工作环境unclassified