2022
DOI: 10.1016/j.polymer.2022.124734
|View full text |Cite
|
Sign up to set email alerts
|

Thermally remendable bismalemide-MWCNT/DA-epoxy nanocomposite via Diels-Alder bonding

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

0
9
0

Year Published

2023
2023
2024
2024

Publication Types

Select...
9

Relationship

0
9

Authors

Journals

citations
Cited by 13 publications
(9 citation statements)
references
References 50 publications
0
9
0
Order By: Relevance
“…51 In the FTIR spectrum of MWCNTs, the peaks at 3554, 3478, 3408, 3140, 1404, and 1129 cm −1 are attributed to the stretching vibrations of –OH and C–O, and the conjugate stretching vibration of CC, respectively. 52 The two peaks at 3483 and 1633 cm −1 in the spectrum of EG are attributed to the stretching vibrations of the single bonds of –OH and CC, respectively. 53 Furthermore, the obvious characteristic peak of PW at 1468 cm −1 was not observed for sample S5.…”
Section: Resultsmentioning
confidence: 99%
“…51 In the FTIR spectrum of MWCNTs, the peaks at 3554, 3478, 3408, 3140, 1404, and 1129 cm −1 are attributed to the stretching vibrations of –OH and C–O, and the conjugate stretching vibration of CC, respectively. 52 The two peaks at 3483 and 1633 cm −1 in the spectrum of EG are attributed to the stretching vibrations of the single bonds of –OH and CC, respectively. 53 Furthermore, the obvious characteristic peak of PW at 1468 cm −1 was not observed for sample S5.…”
Section: Resultsmentioning
confidence: 99%
“…Compared with the PTDA, the peaks showed a redshift, which indicated that the hydrogen-bond interactions were weakened after adding the PEG. In addition, in the inset picture, the typical absorption peak of the DA addition bond represented by succinimide rings occurred at about 1773 cm –1 …”
Section: Resultsmentioning
confidence: 99%
“…In addition, in the inset picture, the typical absorption peak of the DA addition bond represented by succinimide rings occurred at about 1773 cm −1 . 35 As for the SSPCMs, the enthalpy value only comes from PEG, and the PTDA almost has no contribution. 32 The influence of the dynamic crosslinking PTDA network on the crystalline properties and crystal structure of PEG can be characterized via XRD and DSC.…”
Section: Methodsmentioning
confidence: 97%
“…Therefore, these SHEs are typically used at temperatures not exceeding 120 °C. Moreover, the modulus of most of these SHEs is in the range of 1.5–3 GPa, ,,, which is lower than that of engineering epoxy resins. It is worth noting that due to the monotonicity of these DA reactions, the healing temperature and modulus of these SHEs vary over a narrow range.…”
Section: Introductionmentioning
confidence: 90%