The Use of Tannic Acid-Glutaraldehyde in the Study of Elastic and Elastic-Related Fibers

Abstract: Fixation with tannic acid-glutaraldehyde permits distinction of oxytalan, elaunin and elastic fibers in the electron microscope. The results obtained using tannic acid at concentrations of 1.0%, 0.5% and 0.25% in 3% glutaraldehyde were compared. The 0.25% concentration is recommended for studying fine details of connective fibrils and for regular staining of elastin.

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1

Citation Types

1
72
0
5

Year Published

1977
1977
2016
2016

Publication Types

Select...
9
1

Relationship

0
10

Authors

Journals

citations
Cited by 134 publications
(78 citation statements)
references
References 8 publications
1
72
0
5
Order By: Relevance
“…The ventral prostates of control and treated gerbils were processed for transmission electron microscopy as described previously (De Carvalho et al, 1994), employing the fixation procedure of Cotta-Pereira et al (1976). Briefly, tissue fragments were fixed in 0.25% tannic acid plus 3% glutaraldehyde in Millonig's buffer, dehydrated in acetone, and embedded in Araldite resin.…”
Section: Transmission Electron Microscopymentioning
confidence: 99%
“…The ventral prostates of control and treated gerbils were processed for transmission electron microscopy as described previously (De Carvalho et al, 1994), employing the fixation procedure of Cotta-Pereira et al (1976). Briefly, tissue fragments were fixed in 0.25% tannic acid plus 3% glutaraldehyde in Millonig's buffer, dehydrated in acetone, and embedded in Araldite resin.…”
Section: Transmission Electron Microscopymentioning
confidence: 99%
“…Strains were cultured and maintained under 20 C ± 1.50 µmol photons m À2 s À1 irradiance and 14 : 10 h light: dark cycle in the Culture Collection of IBILCE/UNESP. The samples were fixed by immersion in 3 % glutaraldehyde plus 0.25 % tannic acid solution in Millonig's buffer, pH 7.3, containing 0.54 % glucose for 24 h. After washing with the same buffer, they were post-fixed with 1 % osmium tetroxide for 2 h, washed again, dehydrated in a graded acetone series and embedded in Araldite resin (Cotta-Pereira et al, 1976). Ultrathin sections (50-75 nm) were cut using a diamond knife and contrasted with 2 % uranyl acetate for 30 min (Watson, 1958), followed by 2 % lead citrate in sodium hydroxide solution for 10 min (Venable & Coggeshall, 1965).…”
mentioning
confidence: 99%
“…After washing with the same buffer, they were postfixed with 1% osmium tetroxide for 2 hr, washed again, dehydrated in graded acetone series, and embedded in Araldite resin (Cotta-Pereira et al, 1976). Ultrathin sections (range, 50-75 nm) were cut using a diamond knife and contrasted with 2% uranyl acetate for 30 min (Watson, 1958), followed by 2% lead citrate in sodium hydroxide solution for 10 min (Venable and Coggeshall, 1965).…”
Section: Transmission Electron Microscopymentioning
confidence: 99%