The inhibition of pitting corrosion of stainless steels by chromate and molybdate ions

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

6
107
0

Year Published

2007
2007
2022
2022

Publication Types

Select...
8
2

Relationship

0
10

Authors

Journals

citations
Cited by 199 publications
(113 citation statements)
references
References 23 publications
6
107
0
Order By: Relevance
“…49 Pure Mo has been purported to form a protective MoO 2 -based passive film or can generate MoO 4 2-species, which could reduce to the MoO 2 film at pit sites. 50,51 Elemental Mo can also favour pit repassivation in stainless steels. 52 However in HEAs/CCAs, Mo tends to form a Mo and Cr-rich sigma (σ) phase, 53,54 which could remove both Cr and Mo from the alloy matrix.…”
Section: The Influence Of Different Alloying Elements On the Corrosiomentioning
confidence: 99%
“…49 Pure Mo has been purported to form a protective MoO 2 -based passive film or can generate MoO 4 2-species, which could reduce to the MoO 2 film at pit sites. 50,51 Elemental Mo can also favour pit repassivation in stainless steels. 52 However in HEAs/CCAs, Mo tends to form a Mo and Cr-rich sigma (σ) phase, 53,54 which could remove both Cr and Mo from the alloy matrix.…”
Section: The Influence Of Different Alloying Elements On the Corrosiomentioning
confidence: 99%
“…Despite the marked reductions in the occurrence of meta-stable pits by the presence of the inhibitors, stable pitting still occurs. This signifies that not all the sites on the metals are prevented from generating stable pits [50].…”
Section: Effect Of Inorganic Inhibitorsmentioning
confidence: 99%
“…50,51 Furthermore, majority of the metastable pitting activities was observed in the beginning of the experiments and decreased with time, which can be attributed to the decrease of the number of susceptible sites available for metastable pitting. 36,52 ) unless CC License in place (see abstract). The samples after metastable pitting tests were examined using SEM/EDS.…”
Section: Resultsmentioning
confidence: 99%