2022
DOI: 10.1016/j.matpr.2021.12.481
|View full text |Cite
|
Sign up to set email alerts
|

The influence of thickness and final heat treatment on mechanical properties and dimensional stability of binderless fiberboards from steam exploded Arundo donax L

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1
1

Citation Types

0
3
0

Year Published

2023
2023
2023
2023

Publication Types

Select...
2

Relationship

1
1

Authors

Journals

citations
Cited by 2 publications
(3 citation statements)
references
References 22 publications
0
3
0
Order By: Relevance
“…Untreated AD is generally composed of 29.2–43.1% of cellulose, 19.2–24.3% lignin, and 14.5–32.0% of hemicellulose, depending mainly on age [ 45 , 49 , 50 , 51 ]. The STEX process performed has already been described in other papers [ 44 , 45 , 48 ] and the process parameters used in this study were the pre-treatment temperature (Tr) of 200 °C and the time (tr) of 9.5 min.…”
Section: Methodsmentioning
confidence: 99%
See 2 more Smart Citations
“…Untreated AD is generally composed of 29.2–43.1% of cellulose, 19.2–24.3% lignin, and 14.5–32.0% of hemicellulose, depending mainly on age [ 45 , 49 , 50 , 51 ]. The STEX process performed has already been described in other papers [ 44 , 45 , 48 ] and the process parameters used in this study were the pre-treatment temperature (Tr) of 200 °C and the time (tr) of 9.5 min.…”
Section: Methodsmentioning
confidence: 99%
“…The STEX process performed has already been described in other papers [44,45,48] and the process parameters used in this study were the pre-treatment temperature (Tr) of 200 °C and the time (tr) of 9.5 min.…”
Section: Medium Density Fiberboards Manufacturingmentioning